Study of Graphite Content and Sintering Temperature on Wear and Microstructure of Fe+C Powder Metallurgy Preform

1
Atish Sanyal
Atish Sanyal
2
T.K Mishra
T.K Mishra
3
Dr. Manish Choubey
Dr. Manish Choubey
4
Dr. A.C Saxena
Dr. A.C Saxena
1 Gyan Ganga Institute of Technology & Sciences, Jabalpur, Madhya Pradesh

Send Message

To: Author

GJRE Volume 14 Issue A4

Article Fingerprint

ReserarchID

E5756

Study of Graphite Content and Sintering Temperature on Wear and Microstructure of Fe+C Powder Metallurgy Preform Banner
  • English
  • Afrikaans
  • Albanian
  • Amharic
  • Arabic
  • Armenian
  • Azerbaijani
  • Basque
  • Belarusian
  • Bengali
  • Bosnian
  • Bulgarian
  • Catalan
  • Cebuano
  • Chichewa
  • Chinese (Simplified)
  • Chinese (Traditional)
  • Corsican
  • Croatian
  • Czech
  • Danish
  • Dutch
  • Esperanto
  • Estonian
  • Filipino
  • Finnish
  • French
  • Frisian
  • Galician
  • Georgian
  • German
  • Greek
  • Gujarati
  • Haitian Creole
  • Hausa
  • Hawaiian
  • Hebrew
  • Hindi
  • Hmong
  • Hungarian
  • Icelandic
  • Igbo
  • Indonesian
  • Irish
  • Italian
  • Japanese
  • Javanese
  • Kannada
  • Kazakh
  • Khmer
  • Korean
  • Kurdish (Kurmanji)
  • Kyrgyz
  • Lao
  • Latin
  • Latvian
  • Lithuanian
  • Luxembourgish
  • Macedonian
  • Malagasy
  • Malay
  • Malayalam
  • Maltese
  • Maori
  • Marathi
  • Mongolian
  • Myanmar (Burmese)
  • Nepali
  • Norwegian
  • Pashto
  • Persian
  • Polish
  • Portuguese
  • Punjabi
  • Romanian
  • Russian
  • Samoan
  • Scots Gaelic
  • Serbian
  • Sesotho
  • Shona
  • Sindhi
  • Sinhala
  • Slovak
  • Slovenian
  • Somali
  • Spanish
  • Sundanese
  • Swahili
  • Swedish
  • Tajik
  • Tamil
  • Telugu
  • Thai
  • Turkish
  • Ukrainian
  • Urdu
  • Uzbek
  • Vietnamese
  • Welsh
  • Xhosa
  • Yiddish
  • Yoruba
  • Zulu

The present paper investigates the effect of sintering temperature and graphite content on the microstructure and effect on wear and frictional properties of Fe+C powder metallurgy preforms. For the present work the specimens were prepared with graphite content 0.5%, 1%, 1.5% and 2% by weight and were sintered at three sintering temperature 800°C, 900°C and 1050°C. Microstructural properties were evaluated using scanning electron microscopy. The wear and friction property of the powder preforms were tested on Pin-On-Disc apparatus. The powder specimen was used as pins and the disc was of AISI 51200 steel. The experiments was carried out under load of 40 N, speed 1000 rpm, time 1500 seconds and relative humidity 60% -65%. The result was 2% graphite content specimen with sintering temperature 1050°C showed good wear resistance. The wear rate decreased with the increase in sintering temperature and increase in graphite content of the specimen.

Funding

No external funding was declared for this work.

Conflict of Interest

The authors declare no conflict of interest.

Ethical Approval

No ethics committee approval was required for this article type.

Data Availability

Not applicable for this article.

Atish Sanyal. 2014. \u201cStudy of Graphite Content and Sintering Temperature on Wear and Microstructure of Fe+C Powder Metallurgy Preform\u201d. Global Journal of Research in Engineering - A : Mechanical & Mechanics GJRE-A Volume 14 (GJRE Volume 14 Issue A4): .

Download Citation

Journal Specifications

Crossref Journal DOI 10.17406/gjre

Print ISSN 0975-5861

e-ISSN 2249-4596

Classification
Not Found
Version of record

v1.2

Issue date

July 9, 2014

Language

English

Experiance in AR

The methods for personal identification and authentication are no exception.

Read in 3D

The methods for personal identification and authentication are no exception.

Article Matrices
Total Views: 4396
Total Downloads: 2188
2026 Trends
Research Identity (RIN)
Related Research

Published Article

The present paper investigates the effect of sintering temperature and graphite content on the microstructure and effect on wear and frictional properties of Fe+C powder metallurgy preforms. For the present work the specimens were prepared with graphite content 0.5%, 1%, 1.5% and 2% by weight and were sintered at three sintering temperature 800°C, 900°C and 1050°C. Microstructural properties were evaluated using scanning electron microscopy. The wear and friction property of the powder preforms were tested on Pin-On-Disc apparatus. The powder specimen was used as pins and the disc was of AISI 51200 steel. The experiments was carried out under load of 40 N, speed 1000 rpm, time 1500 seconds and relative humidity 60% -65%. The result was 2% graphite content specimen with sintering temperature 1050°C showed good wear resistance. The wear rate decreased with the increase in sintering temperature and increase in graphite content of the specimen.

Our website is actively being updated, and changes may occur frequently. Please clear your browser cache if needed. For feedback or error reporting, please email [email protected]
×

This Page is Under Development

We are currently updating this article page for a better experience.

Request Access

Please fill out the form below to request access to this research paper. Your request will be reviewed by the editorial or author team.
X

Quote and Order Details

Contact Person

Invoice Address

Notes or Comments

This is the heading

Lorem ipsum dolor sit amet, consectetur adipiscing elit. Ut elit tellus, luctus nec ullamcorper mattis, pulvinar dapibus leo.

High-quality academic research articles on global topics and journals.

Study of Graphite Content and Sintering Temperature on Wear and Microstructure of Fe+C Powder Metallurgy Preform

Atish Sanyal
Atish Sanyal Gyan Ganga Institute of Technology & Sciences, Jabalpur, Madhya Pradesh
T.K Mishra
T.K Mishra
Dr. Manish Choubey
Dr. Manish Choubey
Dr. A.C Saxena
Dr. A.C Saxena

Research Journals